Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROLENE® ARPS HI 100-3 Polystyrene Compounded Resin

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPS HI 100-3 Polystyrene Compounded Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 3.0 - 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 - 12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 34.2 MPa
4960 psi
ASTM D638
Flexural Modulus 2.12 GPa
308 ksi
ASTM D790
Izod Impact, Notched 0.801 - 1.07 J/cm
1.50 - 2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved