Aclo Accucomp Polycarbonate POL050L Low Viscosity

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polycarbonate POL050L Low Viscosity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
MD; ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength at Break 62.0 MPa
8990 psi
ASTM D638
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Elongation at Yield 45 %
45 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 8.22 J/cm
15.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F