Material Notes:
Approved to Suzuki PP-S3 Med Grey T01
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 22 g/10 min
22 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 135 %
135 %
ASTM D638
Tensile Modulus 1.00 GPa
145 ksi
ASTM D638
Flexural Strength 35.0 MPa
5080 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
Descriptive Properties Value Comments
Flammability Pass
FMVSS 302