Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
MD; ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
Flexural Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 3.60 GPa
522 ksi
ASTM D790
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F