Aclo Accutech Polypropylene Homopolymer HP0336W30L1 Wollastonite Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0336W30L1 Wollastonite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D638
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 17 %
17 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.899 GPa
420.5 ksi
ASTM D638
Flexural Strength 42.0 MPa
6090 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F