Material Notes:
High impact resistanceInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Conditioned; ISO 868
78
78
ISO 868
Tensile Strength, Yield 40.0 MPa
5800 psi
Conditioned; ISO R 527
60.0 MPa
8700 psi
ISO R 527
Elongation at Yield >= 50 %
>= 50 %
ISO R 527
>= 50 %
>= 50 %
Conditioned; ISO R 527
Modulus of Elasticity 0.700 GPa
102 ksi
Conditioned; ISO 178
2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180/1A
NB
NB
Conditioned; ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
NB
NB
Conditioned; ISO 179/IeU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/IeA
4.00 J/cm²
19.0 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
ASTM E831
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
Conditioned; CEI 60093
1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A