Polymer Property : Modulus of Elasticity = 1.50 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.50 GPa
218 ksi
DIN 53457
Ineos Nova S-3500MG Compact Polystyrene Microgranulates  (discontinued **)
Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and ..
Modulus of Elasticity 1.50 GPa
218 ksi
DIN 53457
Ineos Nova S-4600 High Impact Compact Polystyrene  (discontinued **)
High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection mold..
Modulus of Elasticity 1.50 GPa
218 ksi
DIN 53457
Ineos Nova S-7600MG Compact Polystyrene Microgranulates  (discontinued **)
High impact polystyrene Microgranulates, having a diameter of 0.8 -1.0 mm, especially useful for compounding and extrusion applications. Due to the very high viscosity and the absence of weakener, ..
Modulus of Elasticity 1.50 - 2.60 GPa

@Temperature -18.0 - 71.0 °C
218 - 377 ksi

@Temperature -0.400 - 160 °F
Average value: 2.05 GPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Modulus of Elasticity 1.50 - 1.90 GPa

@Temperature 60.0 - 90.0 °C
218 - 276 ksi

@Temperature 140 - 194 °F
Average value: 1.70 GPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Modulus of Elasticity 1.50 - 3.79 GPa
218 - 550 ksi
Average value: 2.57 GPa Grade Count:39
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Modulus of Elasticity 1.50 - 6.543 GPa

@Temperature -40.0 - 150 °C
218 - 949.0 ksi

@Temperature -40.0 - 302 °F
Average value: 3.47 GPa Grade Count:3
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Modulus of Elasticity 1.50 GPa
218 ksi
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Modulus of Elasticity 1.50 GPa
218 ksi
0°C; ASTM D638
Micropol Isoplas P651 Crosslinkable Polyethylene
Information provided by Micropol Limited
Modulus of Elasticity 1.50 GPa
218 ksi
ISO 527-2
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Modulus of Elasticity 1.50 GPa
218 ksi
MD; ExxonMobil Method
ExxonMobil Metallyte™ UHB 35MU842 OPP Film
Product Description: A metalized high opacity white oriented polypropylene film. It is biaxially oriented, multi-layer polypropylene film with aluminum deposited on an adhesion promoting layer. The ..
Modulus of Elasticity 1.50 GPa
218 ksi
MD; ExxonMobil Method
ExxonMobil Oppalyte™ 36MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa ..
Modulus of Elasticity 1.50 GPa
218 ksi
ISO 178
Addiplast Addilene PMD 50258 Polypropylene Copolymer
For electroplatingInformation provided by Addiplast.
Modulus of Elasticity 1.50 GPa
218 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 ZG30 Nylon 6, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 1.50 GPa
218 ksi
ISO 527-2
BASF Ultraform® N2650 Z4 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Modulus of Elasticity 1.50 GPa
218 ksi
ISO 527-1/-2
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned)
Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c..
Modulus of Elasticity 1.50 GPa
218 ksi
ISO 527
BASF Ultramid® C3U PA66/6 (Conditioned)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.
Modulus of Elasticity 1.50 - 9.50 GPa
218 - 1380 ksi
Average value: 4.46 GPa Grade Count:23
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Modulus of Elasticity 1.50 GPa
218 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 G30 Nylon 6, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast.