Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell BS-10 Nylon 6, General Purpose

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell BS-10 Nylon 6, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0125 cm/cm
0.0125 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 78
78
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Compressive Yield Strength 62.0 MPa
8990 psi
ASTM D695
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648
Flammability, UL94 V-2
V-2