Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly gained recognition in the industry as a high performance material at a similar cost as standard GPO-1. H755 has been successfully sealed tube tested for compatibility in a number of high voltage 220ºC U.L. recognized insulation systems (UL File #E83907 Systems HRP- HV1 and HRP- HV2). There are numerous applications in transformers and motors where a Class F material is required or performance upgrade without cost penalty is desirable. Standard color - Ivory. Meets Gov't Specs - LP-509, I-24768/6.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D572
Water Absorption 0.35 %
0.35 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 48
48
Tensile Strength, Ultimate 76.0 MPa
11000 psi
Flexural Strength 172 MPa
24900 psi
Flexural Modulus 11.0 GPa
1600 ksi
Compressive Strength 276 MPa
40000 psi
Shear Strength 103 MPa
14900 psi
ASTM D732
Izod Impact, Notched 4.50 J/cm
8.43 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Approximate temperature class
Electrical Properties Metric English Comments
Dielectric Constant 4.8

@Frequency 60 Hz
4.8

@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 1.59 mm
508 kV/in

@Thickness 0.0625 in
Perpendicular, Short Time in Oil; ASTM D149
Dissipation Factor 0.020

@Frequency 60 Hz
0.020

@Frequency 60 Hz
ASTM D150
Arc Resistance 150 sec
150 sec
ASTM D495