Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 1.90 GPa
275 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
0.587 J/cm

@Temperature -40.0 °C
1.10 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 11.7 J/cm
22.0 ft-lb/in
ASTM D256
8.01 J/cm

@Temperature -40.0 °C
15.0 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Gardner Impact 1.10 J
0.811 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Users viewing this material also viewed the following: