Aearo E-A-R Specialty Composites VersaDamp™ V-2725 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Aearo E-A-R Specialty Composites
Trade Name VersaDamp™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aearo E-A-R Specialty Composites VersaDamp™ V-2725 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded into a wide variety of standard or custom isolators, including grommets, equipment mounts, bumpers, and gaskets. They feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.Information provided by Aearo E-A-R Specialty Composites.
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
5 sec.; ASTM D2240
Tensile Strength at Break 6.73 MPa
976 psi
ASTM D412
Elongation at Break 381 %
381 %
ASTM D412
Tensile Modulus 0.00379 GPa
0.549 ksi
ASTM D412
Compressive Yield Strength 0.390 MPa
56.6 psi
Compressive Load Deflection at 5%; ASTM D575
0.770 MPa
112 psi
Compressive Load Deflection at 10%; ASTM D575
1.17 MPa
170 psi
Compressive Load Deflection at 15%; ASTM D575
1.66 MPa
241 psi
Compressive Load Deflection at 20%; ASTM D575
2.33 MPa
338 psi
Compressive Load Deflection at 25%; ASTM D575
Compressive Modulus 0.00760 GPa
1.10 ksi
at 15% Compression; ASTM D575
Resilience 35
35
% Bashore Rebound; 22°C; ASTM D2632
50
50
% Bashore Rebound; 70°C; ASTM D2632
Tear Strength 24.9 kN/m
142 pli
ASTM D624
Compression Set 14.5 %
14.5 %
24 hour at 20°C; ASTM D395B
20.1 %
20.1 %
1/2 hour at 20°C; ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Continuous
125 °C
257 °F
Intermittent
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D2137
Flammability, UL94 HB
HB
Meets HBF
Descriptive Properties Value Comments
MVSS 302 Flammability Passes
Relative Peak Transmissibility 11.2 dB
G-411 Grommet; 1.2lb load @ 20°C
Users viewing this material also viewed the following: