Material Notes:
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in pure nickel strip.Homogeneity, microcleanliness, and close composition control enhances weldability.Significantly low levels of surface oxides reduces die wear and provides excellent solderability.Excellent formability.Typical applications for rechargeable batteries: computers, cellular phones, power tools, electric vehicles, pagers, and camcorders.
Physical Properties Metric English Comments
Density 8.90 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B >= 91
>= 91
Hardness, Vickers 193 - 203
193 - 203
Tensile Strength, Ultimate 586 - 589 MPa
85000 - 85400 psi
Tensile Strength, Yield 552 - 655 MPa

@Strain 0.200 %
80100 - 95000 psi

@Strain 0.200 %
Elongation at Break 3.0 - 6.0 %
3.0 - 6.0 %
typical
Poissons Ratio 0.31
0.31
Thermal Properties Metric English Comments
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Melting Point 1453 °C
2647 °F
Component Elements Properties Metric English Comments
Carbon, C 0.0050 - 0.020 %
0.0050 - 0.020 %
Copper, Cu <= 0.0050 %
<= 0.0050 %
Iron, Fe <= 0.050 %
<= 0.050 %
Manganese, Mn <= 0.070 %
<= 0.070 %
Nickel, Ni 99.8 %
99.8 %
Silicon, Si <= 0.0010 %
<= 0.0010 %
Sulfur, S <= 0.0010 %
<= 0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000763 ohm-cm

@Temperature 20.0 °C
0.00000763 ohm-cm

@Temperature 68.0 °F
Curie Temperature 353 °C
667 °F