Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aptek 6500-PMF Electrically conductive epoxy adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Aptek Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aptek 6500-PMF Electrically conductive epoxy adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High purity, low outgassing, electrically conductive adhesiveAPTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic die attach applicationsHigh purity resin system for minimum level of ionic contamination to prevent corrosion problems; High cross-link density to maintain stability and minimize outgassing during operational life even in high-vacuum environments and sealed packages; Smooth thixotropic consistency for machine stamping applications; Viscosity can be factory controlled for screening or dispensing applications; Contains no diluents or solvents to minimize formation of voids during cureInformation provided by Aptek Laboratories, Inc.
Physical Properties Metric English Comments
Density 2.90 g/cc
0.105 lb/in³
ASTM D1475
Viscosity 25000 cP
25000 cP
Spindle #5; 10 rpm; ASTM D1824
Outgassing - Total Mass Loss 0.10 %
0.10 %
Cured property at 125ºC; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.0010 %
0.0010 %
Cured property at 125ºC; at 10E-6 torr; ASTM E595
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
ASTM D2240
Adhesive Bond Strength 15.2 MPa
2200 psi
Al-to-Al Lap Shear; Cured property; ASTM D1002
39.3 MPa
5700 psi
Cured property; Die Shear for Ag to Si, 0.07" x 0.07" IC
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; Perkin Elmer TMS-2
147 µm/m-°C

@Temperature 20.0 °C
81.7 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; Perkin Elmer TMS-2
Glass Transition Temp, Tg 155 °C
311 °F
Cured property; Perkin-Elmer TMS-2
Flash Point >= 150 °C
>= 302 °F
ASTM D92
Electrical Properties Metric English Comments
Volume Resistivity 0.00020 ohm-cm
0.00020 ohm-cm
Cured property; ASTM D257
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Cure 2 hrs
165 °C
329 °F
Cure 2 hrs
Users viewing this material also viewed the following: