Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
ISO 11359
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ASTM D696
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
CTE, linear 45.0 µm/m-°C

@Temperature <=152 °C
25.0 µin/in-°F

@Temperature <=306 °F
Average below Tg; ISO 11359
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
CTE, linear 45.0 µm/m-°C

@Temperature >=149 °C
25.0 µin/in-°F

@Temperature >=300 °F
ASTM E228
Greene Tweed Arlon® 1163 PEEK, Glass Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Alpha 1
Tra-Con Tra-Bond 226U01 High Temperature Controlled Flow Adhesive
TRA-BOND 226U01 is a one-part, controlled flow adhesive with high temperature resistance.Information provided by Tra-Con Inc.
CTE, linear 45.0 µm/m-°C

@Temperature 50.0 - 200 °C
25.0 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 45.0 µm/m-°C

@Temperature 200 - 300 °C
25.0 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; Perkin Elmer TMS-2
Aptek 6500-PMF Electrically conductive epoxy adhesive
High purity, low outgassing, electrically conductive adhesiveAPTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic d..
CTE, linear 45.0 µm/m-°C

@Temperature <=28.0 °C
25.0 µin/in-°F

@Temperature <=82.4 °F
below Tg
Resinlab® EP1200 Black Casting Resin
Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re..
CTE, linear 45.0 µm/m-°C

@Temperature <=27.0 °C
25.0 µin/in-°F

@Temperature <=80.6 °F
below Tg
Resinlab® EP1200LV Casting Resin
Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ISO 11359
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
CTE, linear 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Average below Tg; ASTM D696
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..