Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass

Category Ceramic , Glass
Manufacturer Aremco
Trade Name Aremco-Seal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
Solids Content 54 %
54 %
by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 1000 - 2000 cP
1000 - 2000 cP
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 621 °C
1150 °F
Continuous
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Dry Time 0.5 hour
0.5 hour
Touch
0.5 hour
0.5 hour
Handling
0.5 - 1 hour
0.5 - 1 hour
Recoat
Cure Time 30.0 - 60.0 min
0.500 - 1.00 hour
Air Set prior to curing
30.0 min

@Temperature 621 °C
0.500 hour

@Temperature 1150 °F
Shelf Life 6.00 Month
6.00 Month