Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 41940C020 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 41940C020 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Substrate
508 microns
20.0 mil
Silicone
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property
Tensile Strength 6.89 MPa
1000 psi
Silicone Property
Elongation at Break 450 %
450 %
Silicone Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
E54153
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Brown
Total Product Weight (oz/yd2) 17.6