Material Notes:
1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Design/Construction:Rubber: Cured self-fusing silicone rubberCross-section: 1" wide rectangularInterleave: 2.5 mil PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 762 microns
30.0 mil
Rubber; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 8.69 MPa
1260 psi
Silicone Property; Arlon SQA-TMS-009
10.56 MPa
1531 psi
Product Property; Arlon SQA-TMS-048
Elongation at Break 439 %
439 %
Silicone Property; Arlon SQA-TMS-009
475 %
475 %
Product Property; Arlon SQA-TMS-048
Peel Strength 0.526 kN/m
3.00 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 24.0 kV/mm
610 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red