Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Interleave 1
38.1 microns
1.50 mil
Interleave 2
76.2 microns
3.00 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Side 2; Arlon SQA-TMS-003
102 microns
4.00 mil
Substrate; Arlon SQA-TMS-003
356 microns
14.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Silicone Property; ASTM D2240
Tensile Strength 8.27 MPa
1200 psi
Silicone Property; ASTM D412
Elongation at Break 200 %
200 %
Silicone Property; ASTM D412
Peel Strength 0.596 kN/m
3.40 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 149 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 300 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Blue
Interleave
Blue
Interleave
Red
Total Product Weight (oz/yd2) 13.8
Arlon SQA-TMS-025