Material Notes:
Basic Nylon 6, low viscosity, lubricated.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
24 hrs; ASTM D570
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH; ASTM D570
Water Absorption at Saturation 9.6 %
9.6 %
ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 79.0 MPa
11500 psi
ATSM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 106 MPa
15400 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648
Users viewing this material also viewed the following: