Material Notes:
A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs; ASTM D570
Water Absorption at Saturation 1.1 %
1.1 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 68
68
ASTM D785
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 275 %
275 %
ASTM D638
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Izod Impact, Notched 2.19 J/cm
4.10 ft-lb/in
ASTM D256
0.210 J/cm

@Temperature -40.0 °C
0.393 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 184 °C
363 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ASTM D648