Atom Adhesives AA-BOND F110 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND F110 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. AA-BOND F110 is room temperature system an excellent choice for thin bond-line assembly and repair applications of prisms, lenses and other optic components. And its high strength makes this epoxy ideal for structural applications. AA-BOND F110 exhibits excellent wetting and wicking capabilities which allows it to adhere strongly to glass, ceramics, metals and most rigid plastics.Appearance: Transparent, ClearCure Type: Heat cure or Room TemperatureBenefits:High strengthPerfect insulative propertiesGood resistance to salt solutions, mold acids and Alkalis and many other chemicals Mix Ratio by weight: 100:100/Resin:Hardener Substrates: Excellent choice for thin bond-line assembly and repair applications of prisms, lenses and other optic components. Typical Application: Exhibits excellent wetting and wicking capabilities which allows it to adhere strongly to glass, ceramics, metals and most rigid plastics.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Volatile Organic Compounds (VOC) Content 39.1 g/l
39.1 g/l
uncured
Viscosity 310 cP
310 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Shear Strength 14.8 MPa

@Temperature 25.0 °C,
Time 86400 sec
2150 psi

@Temperature 77.0 °F,
Time 24.0 hour
Lap, Alum to Alum
17.9 MPa

@Temperature 65.0 °C,
Time 3600 sec
2600 psi

@Temperature 149 °F,
Time 1.00 hour
Lap, Alum to Alum
20.7 MPa

@Temperature 65.0 °C,
Time 14400 sec
3000 psi

@Temperature 149 °F,
Time 4.00 hour
Lap, Alum to Alum
Thermal Properties Metric English Comments
CTE, linear 59.9 µm/m-°C
33.3 µin/in-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 90.0 °C
194 °F
Optical Properties Metric English Comments
Refractive Index 1.54
1.54
Transmission, Visible 97 %
97 %
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm
410 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 65.0 °C
1.00 - 2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min
uncured
Descriptive Properties Value Comments
Thixotropic Index 1