Mechanical Properties Metric English Comments
Tensile Modulus 2.58 GPa
374 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Opaque Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.58 GPa
374 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.58 GPa
374 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
Tensile Modulus 2.58 GPa
374 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific)
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Tensile Modulus 2.58 GPa
374 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)
Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance..
Tensile Modulus 2.58 GPa
374 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.58 GPa
374 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East)
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP ABL12 ABS
LNP* Lubricomp* ABL12 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Glass Bead and 5% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.58 GPa
374 ksi
ISO 527-2
Kureha KF Polymer 1300 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East)
Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal
LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
Tensile Modulus 2.58 GPa
374 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS
LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive.
Tensile Modulus 2.58 GPa
374 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM DU242 PEI
Enhanced low temperature impact, high flow Polyetherimide blend. ECO Conforming.
Tensile Modulus 2.58 GPa
374 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66
Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h..
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications.
Tensile Modulus 2.58 GPa
374 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
Tensile Modulus 2.58 GPa
374 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PVX0800 PPE
NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications.
Tensile Modulus 2.58 GPa
374 ksi
Storage
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:..
Tensile Modulus 2.58 GPa
374 ksi
ASTM D-638
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..
Tensile Modulus 2.58 GPa
374 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific)
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.