Material Notes:
20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
ISO 62
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Elongation at Break 7.5 %
7.5 %
ISO 527
Flexural Strength 73.0 MPa
10600 psi
ISO 178
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
1eA; ISO 179
Thermal Properties Metric English Comments
Melting Point 167 °C
333 °F
10°C/min.; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ISO 75
Vicat Softening Point 156 °C
313 °F
50 N; ISO 306
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Constant 4.1

@Frequency 1e+6 Hz
4.1

@Frequency 1e+6 Hz
IEC 60250
4.4

@Frequency 100 Hz
4.4

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243
Dissipation Factor 0.0105

@Frequency 1e+6 Hz
0.0105

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 112
Processing Properties Metric English Comments
Processing Temperature 180 - 230 °C
356 - 446 °F
Barrel temperature
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Users viewing this material also viewed the following: