Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT+PCInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
similar to ISO 62 test
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 61.0 MPa
8850 psi
ISO 527-1
Elongation at Break >= 100 %
>= 100 %
ISO 527-1
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179-1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type PBT+PC