Borealis BS2541 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BS2541 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, and industrial chemical bottles and containers up to 10 liters.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ISO 1183
Environmental Stress Crack Resistance 500 hour
500 hour
Antarox 10%, F50; ASTM D1693-A
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
32 g/10 min

@Load 21.6 kg,
Temperature 190 °C
32 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
50mm/min; ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.10 GPa
160 ksi
1mm/min; ISO 527-2
Flexural Modulus 1.20 GPa
174 ksi
1mm/min; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-2
Processing Properties Metric English Comments
Middle Barrel Temperature 170 - 190 °C
338 - 374 °F
Die Temperature 175 - 190 °C
347 - 374 °F
Melt Temperature 170 - 200 °C
338 - 392 °F