Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Borcoat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression strength.Borcoat BB700E-7032 is recommended as thermal insulation for offshore deep water flow lines.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
At 50 mm/min; ISO 527-2
Elongation at Break <= 200 %
<= 200 %
50 mm/min; ISO 527-3
Tensile Modulus 1.40 GPa
203 ksi
At 1 mm/min; ISO 178
Flexural Modulus 0.800 GPa
116 ksi
At 2 mm/min; ISO 178
Thermal Properties Metric English Comments
Vicat Softening Point 145 °C
293 °F
A (10 N); ISO 306
Processing Properties Metric English Comments
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Melt Temperature 225 - 235 °C
437 - 455 °F
Head Temperature 220 - 230 °C
428 - 446 °F
Users viewing this material also viewed the following: