Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 240 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 215 - 240 °C
419 - 464 °F
Start Point: 225°C
Kingfa FRHIPS-220 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Front Barrel Temperature 215 - 240 °C
419 - 464 °F
Start Point: 225°C
Kingfa FRHIPS-301 Flame Retardant Polystyrene
Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Start Point: 235°C
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LG704W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Injection
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Injection
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Injection
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Injection
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose
Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose
Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance
Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer
INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci..
Front Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer
INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p..
Front Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend
INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by ..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay Technyl® C 206 Nylon 6, EH50
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay TECHNYL® C 216 PA6, DRY
Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY
Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical ..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay TECHNYL® PSB 286 PA6, DRY
Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating
Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Pre-3. Region Temperature
Tisan TISBLEND® PC/ABS
TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Pre-3. Region Temperature
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Chi Mei Acryrex® CM-205 PMMA
High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather ..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Front Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..