Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name Borcoat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie layer between epoxy corrosion protection layer and the top-coat polyethylene, which gives the physical protection of the pipe.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ISO 1183/ISO 1872-2B
Melt Flow 4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ISO 868
Tensile Strength, Yield 18.00 MPa
2611 psi
At 50 mm/min; ISO 527-3
Elongation at Break >= 700 %
>= 700 %
ISO 527-3
Peel Strength >= 4.00 kN/m
>= 22.8 pli
3-layer at 80°C; DIN 30670/NFA 49-710
>= 15.0 kN/m
>= 85.6 pli
3-layer; DIN 30670/NFA 49-710
Thermal Properties Metric English Comments
Melting Point >= 121 °C
>= 250 °F
ISO 3146
Vicat Softening Point 100 °C
212 °F
A50 (10 N); ISO 306
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Users viewing this material also viewed the following: