Borealis Borecene™ RM8402 Linear Polyethylene for Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Borealis
Trade Name Borecene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borecene™ RM8402 Linear Polyethylene for Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borecene RM8402 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Flow and high stiffness make the grade particularly suitable for demanding underground applications. Borecene RM8402 is delivered as pellets.Borecene RM8402 is suitable for rotational molding of products such as tanks for sewerage water and septic purposes, tanks for agricultural purposes, and potable water tanks and underground applications.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
ESCR 10% Igepal® >= 120 hour
>= 120 hour
ARM Method
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
At 50 mm/min; ASTM D683 IV
Flexural Modulus 0.621 GPa
90.0 ksi
At 2 mm/min; ASTM D790
Dart Drop Total Energy 210.0 J/cm
0.3934 ft-lb/mil
(-4oF/-20°C); ASTM D3763
Dart Drop 152 g/micron
3860 g/mil
Instrumented Falling Weight (-4°F/-20°C); ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746