Borealis Borseal™ RE939CF Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Borseal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borseal™ RE939CF Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging, lamination films, and stationary films.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Slip Level 2000 ppm
2000 ppm
EAA; Borealis Method
Mechanical Properties Metric English Comments
Tensile Modulus 0.300 GPa
43.5 ksi
MD/TD; ISO 527-3
Flexural Modulus 0.550 GPa
79.8 ksi
ISO 178
Dart Drop, Total Energy 30.0 J
22.1 ft-lb
900N; ISO 7765-2
Coefficient of Friction >= 0.20
>= 0.20
ISO 8295
Film Tensile Strength at Break, MD 25.0 MPa
3630 psi
ISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa
3630 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 137 °C
279 °F
DSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
ISO 75-2
Vicat Softening Point 116 °C

@Load 1.02 kg
241 °F

@Load 2.25 lb
A50; ISO 306
Optical Properties Metric English Comments
Haze <= 1.5 %
<= 1.5 %
ASTM D1003
Gloss 135 %
135 %
20° of arc; ASTM D2457
Component Elements Properties Metric English Comments
SiO2 0.18 %
0.18 %
Antiblock; Borealis Method
Copyright © lookpolymers.com All Rights Reserved