Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis CG9620 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis CG9620 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CG9620 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Applications: CG9620 is recommended for coated film and co-extrusion applications.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Coating Weight 9.00 g/m²
5.63 lb/ream
BTM 14922
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
DSC; ISO 3146
Descriptive Properties Value Comments
Coating Speed (m/min) > 400 m/min
BTM 14921
Users viewing this material also viewed the following: