Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 131 °C | 268 °F | 10°C/min; ISO 11357-1/-3 |
Yparex 8305 Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melting Point | 131 °C | 268 °F | Exxon Method |
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams |
|||
Melting Point | 131 °C | 268 °F | ISO 3146 |
Total Lacqtene® 2004 TN 52 HDPE pipe
(discontinued **) LACQTENE® 2004 TN 52 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2004 TN 52 is best processed between 190 and 230°C.Informa.. |
|||
Melting Point | 131 °C | 268 °F | |
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Melting Point | 131 °C | 268 °F | |
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Melting Point | 131 - 170 °C | 268 - 338 °F | |
Indium Corp. Indalloy 99 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Global F-8000 High Density Polyethylene Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation. |
|||
Melting Point | 131 °C | 268 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC PM360 HDPE Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Lushan L-5R (HC) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Global S-5000 High Density Polyethylene Description-good for monofilament Applications-ropes, fishing net, agricultural net and sports netInformation provided by Global Polymers Corporation. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357-3 |
Borealis VL4580 High Density Polyethylene VL4580 is a high density polyethylene. This grade is especially designed for monofilament production. Applications: ropes, twines, nets, straps and brushes.Information provided by Borealis AG |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total HDPE XT10 N High Density Polyethylene - Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crac.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357 |
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 4707 EP is a second generation metallocene based High Density Polyethylene with hexene as comonomer.Lumicene® mPE M 4707 EP can be proces.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357 |
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M5220M is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, stress-cr.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E924 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Melting Point | 131 °C | 267 °F | ASTM D3418 |
ExxonMobil HD 6719.17 Injection Molding Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Melting Point | 131 °C | 267 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Pax-Plus™ 3204 Blown Film Resin Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin.. |
|||
Melting Point | 131 °C | 268 °F | Equate Test Method |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |
|||
Melting Point | 131 °C | 268 °F | Equate Test Method |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow DMDA-8907 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE) Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household.. |
|||
Melting Point | 131 °C | 267 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
E-Polymers EFLEX® M300 HDPE M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E927 Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E927ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |