Borealis Daploy™ WB180HMS Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Daploy™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Daploy™ WB180HMS Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Daploy™ WB180HMS is a propylene-based, structurally isomeric polymer.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 - 0.910 g/cc
0.0325 - 0.0329 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Elongation at Yield 38.5 %
38.5 %
ISO 527
Tensile Modulus 1.90 GPa
276 ksi
1mm/min; ISO 527
Flexural Modulus 1.35 GPa
196 ksi
2mm/min; ISO 178
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
A50; ISO 306