Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis HE3366 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis HE3366 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer skin in "foam-skin" constructions. Specifications: ISO 1872-PE; KGHN; 45-D006; ASTM D1248 Type III, Class A, Category 4, Grade E8, E9; the following cable material standards: EN 50290-2-23; DIN VDE 0207, 2YI1; IEC 60708; EN 50407; and DIN VDE 0818.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ISO 1183/ISO 1872-2
Environmental Stress Crack Resistance >= 48 hour

@Temperature 50.0 °C
>= 48 hour

@Temperature 122 °F
Igepal 10%; F20; IEC 60811-4-1/B
Oxidative Induction Time (OIT) 50 min

@Temperature 200 °C
50 min

@Temperature 392 °F
IEC 60811-4-2/B
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
1s; ISO 868
Tensile Strength at Break 23.0 MPa
3340 psi
ISO 527
Elongation at Break 600 %
600 %
ISO 527-2
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
IEC 60093
Dielectric Constant 2.33

@Frequency 1.00e+6 Hz
2.33

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Dissipation Factor 0.000060

@Frequency 1.00e+6 Hz
0.000060

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Processing Temperature 100 - 120 °C
212 - 248 °F
conductor preheating temperature
Melt Temperature 220 - 250 °C
428 - 482 °F
Die Cooling Temperature 50.0 °C
122 °F
water cooling
Descriptive Properties Value Comments
Petroleum Jelly Absorption (%) 5
IEC 60811-4-2
Users viewing this material also viewed the following: