Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product features high impact strength even at sub-zero temperatures and it is suitable for food contact applications due to its excellent organoleptic properties.Applications: Household; low temperature packing; frozen desserts packaging. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
ASTM D792A
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 39
39
ASTM D785
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.600 J/cm

@Temperature -20.0 °C
1.12 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
1.60 J/cm

@Temperature 23.0 °C
3.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ASTM D648
Vicat Softening Point 137 °C
279 °F
10 N; ASTM D1525