Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem EB861/51 Blown Film Extrusion Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem EB861/51 Blown Film Extrusion Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Film for general use; Shrink films; Coextrusion.Additives: Antiblock, DInformation provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM D1505/D792
Thickness 38.0 microns
1.50 mil
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 180 %
180 %
ASTM D882
Film Elongation at Break, TD 1070 %
1070 %
ASTM D882
Elmendorf Tear Strength TD 100 g
100 g
gF; ASTM D1922
Dart Drop Test 140 g
0.309 lb
gF/50%f; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
Optical Properties Metric English Comments
Haze 10 %

@Thickness 0.0380 mm
10 %

@Thickness 0.00150 in
ASTM D1003
Gloss 86 %

@Thickness 0.0380 mm
86 %

@Thickness 0.00150 in
60°; ASTM D2457
Users viewing this material also viewed the following: