Braskem HB 0055 HDPE Blow Molding Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem HB 0055 HDPE Blow Molding Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: 200 liters L-ring drums. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 268 hour

@Thickness 3.00 mm,
Temperature 23.0 °C
268 hour

@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693B
High Load Melt Index 4.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Flexural Modulus 1.254 GPa
181.9 ksi
ASTM D790
Izod Impact, Notched 8.34 J/cm
15.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525