Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 241 MPa
35000 psi
Annealed
483 MPa
70000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 °C
9.00 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.385 J/g-°C

@Temperature 20.0 °C
0.0920 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
Melting Point 1100 °C
2012 °F
Maximum Service Temperature, Air 600 °C
1110 °F
Operating Temperature
Component Elements Properties Metric English Comments
Copper, Cu 94 %
94 %
Nickel, Ni 6.0 %
6.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000997 ohm-cm
0.00000997 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.0005 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.022