Material Notes:
Description: CAPILENE® TU 75 AV is a high melt flow rate, controlled rheology heterophasic copolymer with very high impact strength, even at low temperature. It contains antistatic and nucleating agents allowing fast cycle time even on products with high flow length/wall thickness ratios.Applications: CAPILENE® TU 75 AV is especially designed for fast production of thin wall packaging containers requiring good low temperature impact properties and as base resin for compounding applications. Main applications areas are automotive articles, frozen food packaging, heavy duty technical parts, household articles, closures, garden furniture, garden large containers, pails and tool boxes.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50 mm/min; ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Izod Impact, Notched 0.950 J/cm

@Temperature -20.0 °C
1.78 ft-lb/in

@Temperature -4.00 °F
ASTM D256
4.50 J/cm

@Temperature 23.0 °C
8.43 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 140 °C

@Load 1.02 kg
284 °F

@Load 2.25 lb
ASTM D1525