Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
No. 610 tool steel is an air hardening, high-carbon, high-chromium tool steel having extremely high wear resisting properties. It is very deep hardening, and will be practically free from size change after proper treatment. The high percentage of chromium gives it mild corrosion resisting properties in the hardened condition. It is available as a DeCarb-Free product. DCF bars have been cold-finished in the mill therefore eliminating the need for bar bark removal.Applications: Blanking dies, Forming dies, Coining Dies, Slitting cutters, Heading tools, Long punches, Forming rolls, Edging Rolls, Master tools, Beading tools, Intricate punches, Extrusion dies, Drawing diesInformation provided by Carpenter Technology Corporation.No. 610® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 7.83 g/cc
7.83 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 44 - 45
44 - 45
Tempered at 1200°F
62 - 63
62 - 63
As hardened
Abrasion 37.6
37.6
loss in mm<sup>3</sup>, As-Hardened; ASTM G65
85.9
85.9
loss in mm<sup>3</sup>, Tempered at 1200°F; ASTM G65
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C

@Temperature 20.0 - 100 °C
5.83 µin/in-°F

@Temperature 68.0 - 212 °F
12.2 µm/m-°C

@Temperature 20.0 - 400 °C
6.78 µin/in-°F

@Temperature 68.0 - 752 °F
13.0 µm/m-°C

@Temperature 20.0 - 800 °C
7.22 µin/in-°F

@Temperature 68.0 - 1470 °F
Component Elements Properties Metric English Comments
Carbon, C 1.5 %
1.5 %
Chromium, Cr 12 %
12 %
Iron, Fe 84 %
84 %
As Balance
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 0.80 %
0.80 %
Silicon, Si 0.30 %
0.30 %
Vanadium, V 0.90 %
0.90 %