Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN300HL (Dry) Nylon 66, Heat Stabilized, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN300HL (Dry) Nylon 66, Heat Stabilized, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: General purposeHeat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: