Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Melt blend, FDA approvedCharacteristics: Good processabilityGood drawdown capabilityImproved MVTR propertiesGrease resistanceApplications: MVTR applicationsRelease linersCup stockInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Density 0.943 g/cc
0.0341 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
Condition 190/2.16; ASTM D1238
Neck In 8.60 cm
3.39 in
At 900 fpm
9.50 cm
3.74 in
At 700 fpm
10.2 cm
4.02 in
At 500 fpm
11.1 cm
4.37 in
At 300 fpm
Mechanical Properties Metric English Comments
Coefficient of Friction 0.28
0.28
Poly to poly surface tested
Coefficient of Friction, Static 0.32
0.32
Poly to poly surface tested
Thermal Properties Metric English Comments
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Descriptive Properties Value Comments
MVTR, 100°F 14.9 gms/24hrs/m2
at 100°F