Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Chevron Phillips Chemical Company LP
Trade Name K-Resin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily processed by extrusion and gives thermoformed parts with excellent detail on fast production cycles. Thermoformed parts have greater polystyrene acceptance with equivalent processability, very good clarity, excellent toughness, and good stiffness.Applications: Major applications include thermoformed blister packs, cups and lids, and portion packages.Processing Recommendations:Melt Temperature: 216°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin.Specification Data: When combined with at least 17% food grade polystyrene to produce articles for food contact, KK38 complies with FDA Regulation 21 CFR 177.1640. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50. UL94HB.Data provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ASTM D2240
Tensile Strength, Yield 13.1 MPa
1900 psi
Type 1 @ 2 in/min; ASTM D638
Elongation at Break 180 %
180 %
Type 1 @ 2 in/min; ASTM D638
Flexural Yield Strength 18.6 MPa
2700 psi
ASTM D790
Flexural Modulus 1.055 GPa
153.0 ksi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Impact Test 28.4 J

@Thickness 3.17 mm
20.9 ft-lb

@Thickness 0.125 in
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Vicat Softening Point 76.0 °C
169 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 89 %
89 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature <= 216 °C
<= 421 °F
Users viewing this material also viewed the following: