Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Housewares, Automotive, Tamper Evident Screw Caps for Milk Bottles, Pails (1-2 gallon), Toys, Small Containers for Building CompoundsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
High Load Melt Index 520 g/10 min

@Load 21.6 kg,
Temperature 190 °C
520 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.7 MPa
3580 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 0.970 GPa
141 ksi
3 pt. secant; ASTM D790
1.24 GPa
180 ksi
3 pt. Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -71.0 °C
<= -95.8 °F
ASTM D746