Chevron Phillips Marlex® M368 Polyethylene; Masterbatch

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® M368 Polyethylene; Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This black masterbatch with its medium density polyethylene (MDPE) carrier resin has been formulated for pipe applications that require: Good long-term hoop strengthExtended outdoor lifeClean N550 carbon black Add M368 to the base pipe resin at a 15:1 letdown ratio to achieve a 2.2% carbon black concentration in the pipe.Applications: Information provided by Phillips
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
base resin; ASTM D-1505
0.944 g/cc
0.0341 lb/in³
masterbatch; ASTM D-1505
Carbon Black Loading 35 %
35 %
masterbatch; ASTM D-1603
Melt Flow 5.0 g/10 min
5.0 g/10 min
HLMI, 190/21.6(masterbatch); ASTM D-1238
20 g/10 min
20 g/10 min
HLMI, 190/21.6(base resin); ASTM D-1238