Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm

@Temperature 22.8 °C
14.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 271 - 299 °C
520 - 570 °F
Mold Temperature 65.6 - 79.4 °C
150 - 175 °F
Dry Time 2 - 4 hour

@Temperature 104 °C
2 - 4 hour

@Temperature 220 °F
to ensure moisture content is less than 0.05%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm