Material Notes:
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, instrumentation (industrial and military), missiles, spacecraft, fire and smoke detectors as well as coatings for electronic components, coils and transformers. And no small reason why -- all of the coatings described have been specifically formulated as dielectric insulating coatings to provide the user the ultimate protection available for his electronic assemblies; be it environmental (dirt, dust, humidity, fungus, temperature extremes, etc) or electrical insulation of conductors. These coatings are not designed for use as floor coatings or other general purpose uses; they have been produced under essentially "clean-room" conditions using raw materials with a minimum of ionizable impurities which would detract from their insulating qualities.Cytec (Conap) CC-1191 Acrylic Dielectric Conformal CoatingSingle ComponentPasses Thermal Shock Test (MIL-I-46058C)Non-Nutrient Fungus Resistance (MIL-I-46058C)Passes Flexibility Test (1/8" Mandrel Bend) (MIL-I-46058C)Poor Chemical and Solvent ResistanceSolvent Evaporation Cure Cure Type: Solvent Evaporation
Physical Properties Metric English Comments
Solids Content 30 %
30 %
Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 54.4 °C
130 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Flash Point 18.3 °C
65.0 °F
(TCC)
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity)
1.50e+16 ohm-cm
1.50e+16 ohm-cm
Initial Insulation Resistance (50% Relative Humidity)
2.50e+12 ohm-cm

@Temperature 65.0 °C
2.50e+12 ohm-cm

@Temperature 149 °F
Insulation Resistance During 10th day Cycling (95% Relative Humidity)
Dielectric Constant 3.15
3.15
ASTM D150
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Dissipation Factor 0.010

@Frequency 1e+6 Hz
0.010

@Frequency 1e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 25.0 °C
0.333 hour

@Temperature 77.0 °F
tack free
60.0 min

@Temperature 60.0 °C
1.00 hour

@Temperature 140 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Shelf Life 12.0 Month
12.0 Month
Shelf Life Time at 25°C in original, unopened containers.