Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® 46HF5041LW (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow, Low Warpage (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Flame Retarded + Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® 46HF5041LW (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow, Low Warpage (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.1 %
1.1 %
50% RH / 23°C; Similar to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527-1/-2
Elongation at Break 1.3 %
1.3 %
ISO 527-1/-2
Tensile Modulus 16.0 GPa
2320 ksi
ISO 527-1/-2
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
ISO 75-1/-2
UL RTI, Electrical 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL746B
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
Users viewing this material also viewed the following: