Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.6 MPa
2700 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 0.689 GPa
99.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648