PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Water Absorption 0.070 %
0.070 %
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 103 MPa
15000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 6.89 GPa
1000 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.60 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Annealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
380 °F
Annealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 227 - 249 °C
440 - 480 °F
Molding
Mold Temperature >= 93.3 °C
>= 200 °F
Drying Temperature 107 °C
225 °F
Dry Time 2 hour
2 hour
Descriptive Properties Value Comments
Product Form Pellets